Jingkun: providing you with innovative Guar products
         for Construction Application
Jingkun Chemistry Company, one of the leading
manufacturers for guar derivative products in the
world, serves a wide range of markets including
Construction. We supply our customers with
innovative guar products in their production for
cost effective, better performance and being
environmental friendly.




                 Guar ether : Superior Water-retention agent
                               Thickener & Rheology-modifier
                                     Guar Gum is a polysaccharide extracted from the
                                     seeds of the guar beans, grown in Southern Asia
                                     for centuries. Jingkun has been souring the unique
                                     material from this region for 20 years, controlling
                                     each stage of the extraction and processing to
                                     assure consistent quality.
                                     The exceptional properties of this biocompatible and
                                     renewable plant are the basis for Jingkun’s guar
                                     ether products for construction industry.
What is HPG?
Guar gum is extracted from the seed of the leguminous
shrub of Cyamposis tetragonoloba. Leguminous is
cultivated in the semiarid region of tropical countries
particular in India/ Pakistan. It is usually found in the form
of "splits", that are the endosperms of the seed derived from
the husk and from the inner proteinic part. Guar gum in the form
of powder of different particle size, which is obtained from
the splits by milling.

Hydroxypropyl guar gum (HPG) is synthesized by the
etherification reaction with nonionic propylene oxide
reagent with guar gum. This modification can significantly
improve the important properties of unmodified gum like
alkaline stability, hydrophobicity, solubility, biostability etc.
in context to their application in construction application.

The adequate degree of molar substitution in HPG lead to excellent water retention properties,
which is most important parameter in most of the construction application. The HPG improve
the performance / workability when typically applied in tile adhesives, tile grouts, cement based
wall putty, cement / gypsum based plaster, cement based texture plaster, cement / gypsum
based crack filler, flooring and leveling compound etc.
Due to its excellent thickening efficiency and pseudo plastic rheology behavior, this product
also helps to improve the sag resistance of plaster/ mortar when apply on vertical wall.
Characteristics of HPG


Water retention
Water retention in most of the building materials is one of the most important parameters.
It gives the capability of the mixture to maintain water inside, by allowing a better setting of the
binder and reducing the unpleasant effects of the plastic shrinking.

As per the picture showed, we made two sets of mortar.
One containing HPG JK-705, and one without.
Place same weighted quantity of two mortar separately
on a filter paper.
The filter paper absorbs the water from the mortar
without JK-705; while the mortar containing JK-705
remains the water inside for a long time.
In this case, JK-705 shows good water retention ability
when it applied in the mortar.




                                                                   Mortar with     Mortar without
                                                                   HPG K-705       HPG JK-705
Characteristics of HPG


Consistency
Consistency is an important parameter to avoid the plaster sagging and improve the resistance
to the tile sagging when applied on the vertical wall.

As per the picture showed, we made two sets of mortar.
One containing HPG JK-705, and one without.
The mortar contains the JK-705 gives good standing
and still strength on spatula while another mortar
straight runs out from the spatula.




                                                              Consistency test
Characteristics of HPG


Rheology modifying

The water contain in the mortar acts as lubricants for the solid particles when mortar is spread
on the surface of the objects to which it is applied. The proper amount of water gives mortar the
“ pastiness” or “ creaminess” which is suitable for uniform and easy application.

This rheological characteristic of the final mortar mixture are very important and it depends on
the kind and amount of different ingredients used in the mortar.
The simple mixture of cement, sand and water is not suitable for use as a good mortar because
of the lack of the above rheological characteristics and also because of its poor processing.

This problem can be overcome by selecting the additives used in the formulation of mortars
which act as a both water retention aid and rheology modifier.

This additive is HPG, which exhibits the specific characteristic of bonding and coordinating a
large amount of water once they are dissolved in water.
Why Choose HPG?


  ●   Compared with cellulose ether, HPG is easier to soluble in water.

  ● Due to similar water retention ability, HPG can replace cellulose ether with
  x equal quantity for application of low viscosity & small dosage.

  ● For application of high viscosity & big dosage, HPG can’t completely
  x replace cellulose ether. But use HPG together with cellulose ether can get
  x better performance.

  ● When applied in gypsum based mortar, HPG can distinctly enhance
  x workability and ease of application.

  ● When applied in cement based mortar, HPG can replace cellulose ether with
  x equal quantity. HPG can endow cement based mortar with better anti-sagging,
  x thixotropy and ease of application.

  ●   Due to its cheaper price, end-users can get considerable cost-cutting.
Applications of HPG


Dry cement based wall putty

HPG has good compatibility with different ingredients.
It shows good dispersibility without lump formation, excellent water retention & open time.

HPG enhances workability and ease of application of the final mixture.
And HPG helps the final mixture get outstanding adhesion, good whiteness index, Smooth
finishing etc.

                     Cement based wall putty formulation:

                     No.    Ingredients                            Wt %

                     1.    White Cement                           25 ~ 27
                     2.    Dolomite (400-500 mesh)                45 ~ 50
                     3.    Calcite (400-500 mesh)                 10 ~ 15
                     4.    Calcium Carbonate (400-500 mesh)       10 ~ 12
                     5.    HPG JK-705                             0.6 ~ 0.8
                     6.    Redispersible Polymer Powder           1.8 ~ 2.2
                     7.    Cellulose Fiber                        0.1 ~ 0.2
                     8.    Tartaric Acid                          0.1 ~ 0.2
Applications of HPG


Gypsum based plaster

Thanks to its good water retention ability, HPG improves setting time property & open time of
the final mixture to get outstanding workability with good finishing using hand plaster.
HPG also shows satisfactory adhesion & strength.




                     Gypsum based plaster formulation:

                     No.    Ingredients                           Wt %

                     1.    Gypsum                                  73.5
                     2.    Calcium Carbonate (400-500 mesh)        24.5
                     3.    HPG JK-704                              0.5
                     4.    Redispersible Polymer Powder            1.5
Applications of HPG


Gypsum based crack filler

HPG helps to get excellent ease of application with knife applicator and provides good
smoothness, strength and finishing.




                     Gypsum based crack filler formulation:

                     No.    Ingredients                           Wt %

                     1.    Gypsum                               81.5 ~ 92.5
                     2.    Calcium Carbonate (400-500 mesh)          5 ~ 15
                     3.    HPG JK-704                                   0.5
                     4.    Redispersible Polymer Powder                 1.5
Applications of HPG


Tile adhesives

HPG enhances the adhesion strength, open time as well as adjustable time of the final mixture.
It also helps to improve the workability and ease of application of the final mixture.




                     Tile adhesives formulation:

                     No.    Ingredients                           Wt %

                     1.    Portland cement                         35
                     2.    River sand ( 0.2~0.4 mm )               62.9
                     3.    HPG JK-705                              0.5
                     4.    Redispersible Polymer Powder            1.6
Applications of HPG


Tile grouts

Due to its high open time property, HPG helps to enhance flow as well as leveling and finishing
of the final mixture.
HPG also helps in adhesion strength.




                     Tile grouts formulation:

                     No.    Ingredients                            Wt %

                     1.    Portland cement                           45
                     2.    Minerals                               50~55
                     3.    HPG JK-705                                0.5
                     4.    Redispersible Polymer Powder              1.5
Applications of HPG

Waterborne paints

Rheology modifier is an important additive for paint.
it provides:

    ●   Adequate viscosity
    ●   Impact how thick the paint goes on the how well it flows out when applied
    ●   Resist spattering when applied by roller
    ●   Flow out smoothly


Jingkun specially developed HPG JK-701S for paint application.

JK-701S is prepared by the etherification reaction of nonionic propylene oxide reagent with guar
under alkaline conditions.
Such modification greatly improves some specific properties of native guar like electrolyte
compatibility, stability, solubility, and the rheological characteristics in context to their
utilization in various types of water borne coatings.
Applications of HPG

Waterborne paints                   Important Properties of HPG JK-701S:

  ●   Chemical Name:                Hydroxypropyl guar gum
  ●   CAS No.:                      32491-75-5
  ●   Solubility:                   Excellent cold and hot water
  ●   Rheology in water:            Non-Newtonian pseudoplastic
  ●   Dispersibility in water:      Dispersible with manual stirring. Controlled viscosity development
                                    to allow ease of dispersion and prevention of lump formation.


                         Waterborne paint formulation:

                         No.      Ingredients                                  Wt %

                         1.      Titanium oxide                                 5.0
                         2.      Talc                                           31.0
                         3.      Sodium hexametaphosphate ( 10% solution)       1.5
                         4.      Water                                          11.8
                         5.      Biocide                                        0.3
                         6.      Emulsion ( 54% solids)                         34.4
                         7.      HPG JK-701S ( 2% solution)                     16.0
Applications of HPG

Waterborne paints

Performance of HPG JK-701S VS. conventional rheology modifier HEC in formulation:

   Wet paint testing

   Parameter                        HEC         JK-701S

   Non volatile matter ( %)         50.2          50.5
   Weight/ Liter ( KG/L)            1.13          1.13
   Hiding power ( M2/ L)            4.7           5.2
   Settling ( after 7 days)          Nil          Nil
   Fungal growth ( after 7 days)    Nil            Nil


   Dry film testing

   Parameter                        HEC                  JK-701S

   Visual observation              Comparable        Comparable
   Chalking                          Nil                Nil
   Wet abrasion ( 100 cycles)      Comparable        Comparable
   UV resistance ( 100 hours)      No change         No Change
Applications of HPG

Waterborne paints

After conducting various trials, it was found that JK-701S serves as an ideal substitute for products
like HEC and other rheological additive on account of its following outstanding properties:

    ● Requires less energy for dispersion and imparted similar if not better rheological properties

    p with a distinct economic advantage.
    ●   Ease of incorporation into paint formulation.
    ●   Excellent color development and color acceptance.
    ●   Compatibility with a broad range of paint ingredients.

    ●   Compatible with different electrolytes present in paint formulations.

    ●   Forms highly viscous, homogenous colloidal dispersions when added to cold water.

    ●   Very low water insolubles.

    ●   Excellent resistance to shear degradation.

    ●   Solution is stable at wide range of alkaline pH.
                                      Application Guide

                                Paint             Gypsum based mortar                     Cement based mortar
                         Waterborne     Latex     Tile     Crack                 Tile        Crack       Brick    Wall
Product/ INCI name                                                   Plaster
                          coating       paint   adhesive    filler             adhesive       filler   adhesive   putty

  JK-701/JK-701S
Hydroxypropyl guar gum     √
                           √√           √
                                        √√                            √
  JK-702/JK-702S
Hydroxypropyl guar gum     √
                           √            √
                                        √         √         √         √
                                                                      √
       JK-703
Hydroxypropyl guar gum     √            √        √
                                                 √         √
                                                           √         √
                                                                     √√                                           √
       JK-704
Hydroxypropyl guar gum                          √
                                                √√         √
                                                           √√        √
                                                                     √√          √
                                                                                 √            √
                                                                                              √          √ √
                                                                                                         √ √√
       JK-705
Hydroxypropyl guar gum                          √
                                                √√         √
                                                           √√         √
                                                                      √         √
                                                                                √√           √
                                                                                             √√         √
                                                                                                        √√        √
                                                                                                                  √√



                  √Suitable                 √
                                            √    Recommended            √
                                                                        √√      Highly Recommended
                                                  JK-701
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-701 is nonionic hydroxypropyl guar derived from natural guar gum. It is developed to be applied in water paints,
latex paints.
JK-701 has a special rheology, which allows the user to reduce the sagging and spattering problems of paint products.
And it guarantees an excellent viscosity to improve film building and resist spattering of paint products.
We recommend the usage of JK-701 is determined by your own formulation. The normal usage level in paint is 0.3% to
1.0%.

Specifications:
             Chemical description                                 Nonionic etherified guar gum
             Appearance                                           Ivory fine powder
             Moisture                                             8% Max
             Particle Size through US 60 Mesh                     99.9% Min
                           through US 120 Mesh                    99.0% Min
             Viscosity ( mPa.s)
                                                                  23000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                             5.0~ 7.0

Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                 JK-701S
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-701S is nonionic hydroxypropyl guar derived from natural guar gum. It is developed to be applied in water paints,
latex paints.
JK-701S has a special rheology, which allows the user to reduce the sagging and spattering problems of paint products.
And it guarantees an excellent viscosity to improve film building and resist spattering of paint products.
In order to facilitate its dispersion in water, solubility of JK-701S is delayed by a surface treatment.
To develop its full viscosity, it is necessary to raise the solution pH up to 8~10, with a suitable alkali.
We recommend the usage of JK-701S is determined by your own formulation. The normal usage level in paint is 0.3%
to 1.0%.

Specifications:
             Chemical description                                 Nonionic etherified guar gum
             Appearance                                           Ivory fine powder
             Moisture                                             8% Max
             Particle Size through US 60 Mesh                     99.9% Min
                           through US 120 Mesh                    99.0% Min
             Viscosity ( mPa.s)
                                                                  23000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                             5.0~ 7.0

Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                   JK-702
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-702 is nonionic hydroxypropyl guar derived from natural guar gum. It is developed to be used for thickening and
water-retention in the production of gypsum and plasters.
JK-702 has high molecular weight and very high molar substitution which makes it’s suitable for alkaline conditions, like
a mixture of gypsum-lime and lime cement.
JK-702 to be used alone or in combination with the cellulose ethers has to be determined by your own formulation.

Specifications:
             Chemical description                                   Nonionic etherified guar gum
             Appearance                                             Ivory fine powder
             Moisture                                               8% Max
             Particle Size through US 60 Mesh                       99.9% Min
                           through US 120 Mesh                      99.0% Min
             Viscosity ( mPa.s)
                                                                    15000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                               5.0~ 7.0

Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                 JK-702S
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-702S is nonionic hydroxypropyl guar derived from natural guar gum. It is developed to be used for thickening and
water-retention in the production of gypsum and plasters.
JK-702S has high molecular weight and very high molar substitution which makes it’s suitable for alkaline conditions,
like a mixture of gypsum-lime and lime cement.
In order to facilitate its dispersion in water, solubility of JK-702S is delayed by a surface treatment.
To develop its full viscosity, it is necessary to raise the solution pH up to 8~10, with a suitable alkali.
JK-702S to be used alone or in combination with the cellulose ethers has to be determined by your own formulation.

Specifications:
             Chemical description                                   Nonionic etherified guar gum
             Appearance                                             Ivory fine powder
             Moisture                                               8% Max
             Particle Size through US 60 Mesh                       99.9% Min
                           through US 120 Mesh                      99.0% Min
             Viscosity ( mPa.s)
                                                                    15000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                               5.0~ 7.0
Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                   JK-703
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-703 is nonionic hydroxypropyl guar derived from natural guar gum. It is developed to be used for thickening and
water-retention in the production of gypsum and plasters.
JK-703 has high molecular weight and very high molar substitution which makes it’s suitable for alkaline conditions, like
a mixture of gypsum and lime.
JK-703 to be used alone or in combination with the cellulose ethers has to be determined by your own formulation.

Specifications:
             Chemical description                                   Nonionic etherified guar gum
             Appearance                                             Ivory fine powder
             Moisture                                               8% Max
             Particle Size through US 60 Mesh                       99.9% Min
                           through US 120 Mesh                      99.0% Min
             Viscosity ( mPa.s)
                                                                    10000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                               5.0~ 7.0

Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                  JK-704
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-704 is nonionic hydroxypropyl guar derived from natural guar gum. It is developed for the applications of cement
based plaster, gypsum based plaster.
JK-704 has a special rheology and allows the users to reduce the sagging problems both of cement and gypsum based
products.
JK-704’s high molar substitution guarantees its excellent stability of performance under alkaline conditions, so it is
suitable for gypsum plasters having strong alkaline pH due to lime content.
JK-704 to be used alone or in combination with the cellulose ethers has to be determined by your own formulation.

Specifications:
             Chemical description                                  Nonionic etherified guar gum
             Appearance                                            Ivory fine powder
             Moisture                                              8% Max
             Particle Size through US 60 Mesh                      99.9% Min
                           through US 120 Mesh                     99.0% Min
             Viscosity ( mPa.s)
                                                                   9000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                              5.0~ 7.0
Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months
                                                  JK-705
Chemical name: Hydroxypropyl Guar
CAS Number: 32491-75-5
Applications:
JK-705 is nonionic hydroxypropyl guar derived from natural guar gum. It is developed for the applications of cement
based plaster, gypsum based plaster.
JK-705 has a special rheology and allows the users to reduce the sagging problems both of cement and gypsum based
products.
JK-705’s high molar substitution guarantees its excellent stability of performance under alkaline conditions, so it is
suitable for gypsum plasters having strong alkaline pH due to lime content.
Compared to JK-704, JK-705 has a higher substitution lever, which makes it work better in water retention.
JK-705 to be used alone or in combination with the cellulose ethers has to be determined by your own formulation.

Specifications:
             Chemical description                                  Nonionic etherified guar gum
             Appearance                                            Ivory fine powder
             Moisture                                              8% Max
             Particle Size through US 60 Mesh                      99.9% Min
                           through US 120 Mesh                     99.0% Min
             Viscosity ( mPa.s)
                                                                   7000 Min
             (25 ℃, 2.0% solution, Brookfield, 4# 20 RPM) )
             pH value                                              5.0~ 7.0
Packing: 25Kg net weight, multiwall bag lined with PE bag.
Shelf Life: 12 months

				